Product Details:
Application:industry
Shape:powder
Chemical Composition:Scandium
Description:
Product DescriptionPosition Type of Working Layer Grit Working Procedure RPMg/min Feed Speed (mm/min) Removal
mm
Pos.0 Meter sintered, Segmented 30/40 Chamforing 4500 500-600shape
Pos.1 Meter sintered, Segmented 30/40 Shaping 4500 500-600shape
Pos.2 ABR hot pressed, Continous 70/80 Coarse finishing 4500-46001000-1400 0.3 /-0.05
Pos.3 ABR hot pressed, Continous 140/170 Medium finishing 4500-46001000-1400 0.2 /-0.05
Pos.4 ABR hot pressed, Continous 230/270 Finishing 1200-1500600-800 0.1 /-0.05
Pos.5 ABR hot pressed, Continous 400 Good finishing 1200-1500600-800 0.05 /-0.025
Pos.6 ABR hot pressed, Continous 800 Polishing 1200-1500 600-8000.05 /-0.025
Pos.7 ABR hot pressed, Continous 1500 Polishing and buff 1200-1500600-800 0.05 /-0.025
Pos.8 ABR hot pressed, Continous 3000 Polishing and buff 1200-1500600-800 0.05 /-0.025.
Cnc Wheel